DSC OIT Test Machine

A5D Differential Scanning Calorimeter IPL DSC A5D

DSC / OIT Test machine

Buy price of Differential Scanning Calorimeter test machine

KeyFuture:

Operating in ranges of • ±10, ±20, ±40, ±100, ±160, ±200 mW, with automatic scaling capability
Signal accuracy (normal tests 0.01mW) with the ability to decrease or increase depending on user needs and test type – Selectable signal accuracy from 0.00001 watts to 0.1 milliwatts. Depending on user needs
Calibrated temperature: 0 ~ 550 ° C – maximum up to 550 degrees.
Long-term stable temperature accuracy: 0.1°C.
Heating rate: 20°C/min. (selectable range)
Gas flow: 0-100 ml/min (can be increased/decreased as desired)
Manual gas flow control system with manometer – Inlet gas pressure: 0.2MPa.
Aluminum pen holder 6.7 mm x 2.5 mm –
Machine size: 400x300x250mm.
Temperature range: Room temperature to 550°C – Relative humidity: 55 ~ 75%.
Equipped with a 3.5-inch full-color screen – equipped with touch – no need to connect to a computer
Advanced software under Windows from XP to 11, ability to receive report output in PDF format
Fully vacuum furnace, equipped with 2 inlets with automatic gas selection and one outlet for the exit of the test gas.
Equipped with advanced chips with full 24-bit resolution,
Ability to change resolution for highly accurate tests
Complies with all required international and domestic standards.
No domestic competitor in terms of quality, price, software features, and completely realistic display of sample behavior without any software modification.
With very special software features that are the result of years of interaction with users and the needs assessment of analysts and DSC device users in laboratories, the software has been added, and few devices in the world have those features.